Description

Polyether block amide Pebax® MV 2080 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.

Pebax® MV 2080 resin is an inherently dissipative polymer and can be dry blended or compounded with an isolative polymer to lower the surface resistivity. Refractive index according to an internal method is 1.502.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.07 g/cm³

Show Supplier Material materials with Density of 1.07 g/cm³

dry

ISO 1183

Moisture absorption

1.4 %

Show Supplier Material materials with Moisture absorption of 1.4 %

Sim. to ISO 62

Water absorption

48 %

Show Supplier Material materials with Water absorption of 48 %

Sim. to ISO 62

Mechanical

PropertyValueConditionTesting StandardComment

Elastic modulus

0.08 GPa

Show Supplier Material materials with Elastic modulus of 0.08 GPa

cond.

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min.

Hardness, Shore D

40 [-]

Show Supplier Material materials with Hardness, Shore D of 40 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy unnotched

No Break at 23 and -30°C

dry and cond.

ISO 179/1eU

Thermal

PropertyValueConditionTesting StandardComment

Melting point

160 °C

Show Supplier Material materials with Melting point of 160 °C

dry

ISO 11357-1/-3

10°C/min

Electrical

PropertyValueConditionTesting Standard

Surface resistivity

1e+07 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+07 Ω/sq

cond.

IEC 60093

Volume resistivity

1e+07 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+07 Ω·cm

cond.

IEC 60093

Technological properties

Property
Application areas

Permanent Antistatic Solutions,Permanent Antistatic Solutions E&E

Processing methods

Injection Molding:

  • Typical melt temperature (Min / Recommended / Max): 200°C / 240°C / 270°C.
  • Typical mold temperature: 25–60°C.
  • Drying time and temperature (only necessary for bags opened for more than two hours): 4-6 hours at 65-75°C.


    Extrusion:

  • Typical melt temperature (Min / Recommended / Max): 210°C / 220°C / 230°C.
  • Drying time and temperature (only necessary for bags opened for more than two hours): 4-6 hours at 65-75°C.