Platamid® H 106 Powder

Alternative and trade names
PA*
Want to keep this datasheet? Save it now in your required format

Description

Platamid® H 106 Powder Copolyamide Hot Melt Adhesive / Textile Applications

Platamid® H 106 Powder is a very low melt copolyamide adhesive powder for the production of fusible interlinings.

Platamid® H 106 Powder is particularly useful where bonding temperature low and short bonding time are required for sensitive shell fabrics.

Platamid® H 106 Powder has an excellent dry cleaning resistance and washing resistance up to 40°C.

This product is available in different grain sizes:

  • Platamid®< H 106 PA 100
  • Platamid® H 106 PA 80 (0-80 μm)- Platamid® H 106 PRA 200/25 (0-200 μm)- Platamid® H 106 PTA 120 (0-120 μm)- Platamid® H 106 PTA 170 (80-170 μm)- Platamid® H 106 PTA 170/20 (0-70 μm)- Platamid® H 106 PA 80 Black- Platamid® H 106 PA 80 Red- Platamid® H 106 PRA 170- Platamid® H 106 PTA 170 Black- Platamid® H 106 PTA 170 Red- Platamid® H 106 PTA 60/150

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Thermal

    PropertyValueComment

    Melting point

    115 °C

    Show Supplier Material materials with Melting point of 115 °C

    ISO 11357-1/-3, 10°C/min

    Rheological Properties

    PropertyValueComment

    Melt volume-flow rate

    90 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 90 cm³/10min

    ISO 1133, 160°C/2.16kg

    Technological properties

    Property
    Other

    PACKAGING

    All grades are delivered in 20 kg sealed bags.Platamid® H 106 PA 80 is also delivered in 500 kg sealed big bags (GRVS). These grades are ready to be processed.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.