Platamid® H 2513 Powder

Alternative and trade names
PA*
Want to keep this datasheet? Save it now in your required format

Description

Copolyamide Hot Melt Adhesive / Textile Applications

Platamid® H 2513 Powder is a medium melt viscosity copolyamide adhesive powder for the production of fusible interlinings.

Platamid® H 2513 Powder offers an excellent laundry resistance up to 60°C and an excellent resistance to all kind of steam treatment.

This product is available in different grain sizes:

  • Platamid® H 2513 PA 80 (0-80 μm paste dot)- Platamid® H 2513 PTA 170/20 (0-170 μm powder dot)- Platamid® H 2513 PTA 170 (80-170 μm double dot)

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Thermal

    PropertyValueComment

    Melting point

    128 °C

    Show Supplier Material materials with Melting point of 128 °C

    ISO 11357-1/-3, 10°C/min

    Rheological Properties

    PropertyValueComment

    Melt volume-flow rate

    30 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 30 cm³/10min

    ISO 1133, 160°C/2.16kg

    Technological properties

    Property
    Other

    PACKAGING

    Platamid® H 2513 PTA 170 is delivered in 20 kg sealed bags and 500 kg sealed big bags (GRVS). Platamid® H 2513 PA 80 and Platamid ® H 2513 PTA 170/20 are delivered in 20 kg sealed bags.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.