Description

Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® H 2519 is a thermoplastic co-polyamide hot melt adhesive available in pellet form. This medium melt viscosity, fast re-crystallizing grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.

Platamid® H 2519 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal, natural fibers, etc). In addition,

Platamid® H 2519

also exhibits strong adhesion onto rigid and plasticized PVC as well as ABS, epoxy resin, PU, etc. Dense layers of

Platamid® H 2519

are known to have barrier properties against PVC plasticizer migration.

Platamid® H 2519 is also characterized by a high content of Bio Based Carbon, making it a bio based solution to difficult-to-solve bonding problems.

This product is available:

  • Dried (H 2519 T)
  • Un-dried (H 2519 F)

    PACKAGING

    Platamid® H 2519 T is delivered in 25 kg sealed bags. Platamid® H 2519 F is delivered in 25 kg sealed bags, 500 kg sealed big bags (GRVS or GRVS ALU) and 500 kg sealed rigid containers (GRVC).These grades are ready to be processed.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.

    RENEWABLE CARBON: 50 %

  • This material data has been provided by Arkema Technical Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueConditionTesting Standard

    Bio-based content

    50 %

    Show Supplier Material materials with Bio-based content of 50 %

    Density

    1.09 g/cm³

    Show Supplier Material materials with Density of 1.09 g/cm³

    dry

    ISO 1183

    Rheological Properties

    PropertyValueConditionTesting StandardComment

    Melt volume-flow rate

    8 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 8 cm³/10min

    dry

    ISO 1133

    160°C/2.16kg