Platamid® HX 2544

Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® HX 2544 is a standard thermoplastic co-polyamide hot melt adhesive available in pellet form. This very low melt viscosity grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.

Platamid® HX 2544 offers a good adhesion at low fusing conditions to various polar substrates (thermoplastics, thermosets, metal natural fibers, and more).

Platamid® HX 2544 has good dry cleaning resistance and washing resistance up to 60°C.

This product is available:

  • Dried with optical brightener (HX 2544 TA)
  • Un-dried with optical brightener (HX 2544 FA)

    PACKAGING

    Platamid® HX 2544 TA is delivered in 25 kg sealed bags. Platamid® HX 2544 FA is delivered in 25 kg sealed bags. These grades are ready to be processed.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.

    RENEWABLE CARBON CONTENT=25%

    (calculated, ASTM D6866)

  • This material data has been provided by Arkema Technical Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueConditionTesting Standard

    Bio-based content

    25 %

    Show Supplier Material materials with Bio-based content of 25 %

    Density

    1.01 g/cm³

    Show Supplier Material materials with Density of 1.01 g/cm³

    dry

    ISO 1183

    Thermal

    PropertyValueConditionTesting StandardComment

    Melting point

    95 °C

    Show Supplier Material materials with Melting point of 95 °C

    dry

    ISO 11357-1/-3

    10°C/min

    Rheological Properties

    PropertyValueConditionTesting StandardComment

    Melt volume-flow rate

    104 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 104 cm³/10min

    dry

    ISO 1133

    160°C/2.16kg

    Technological properties

    Property
    Application areas

    Hot Melt Hot Melt Adhesives Flooring - Flooring,Hot Melt Hot Melt Adhesives Interlining / Garments - Interlining / Garments,Textile - Others