Platamid® HX 2592

Alternative and trade names
PA*
Want to keep this datasheet? Save it now in your required format

Description

Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® HX 2592 is a specialty thermoplastic co-polyamide hot melt adhesive available in pellet form. This low to medium melt viscosity grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.

Platamid® HX 2592 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, and more). In addition,

Platamid® HX 2592

also exhibits strong adhesion onto rigid and plasticized PVC as well as ABS, epoxy resin, PU etc. Dense layers of Platamid® HX 2592

are known to have barrier properties against PVC plasticizer migration.

Platamid® HX 2592 is also characterized by a very high content of Bio based Carbon (80%), making it a bio based solution to difficult-to-solve bonding problems.

This product is available:

  • Dried (HX 2592 T)
  • Un-dried (HX 2592 F)

    PACKAGING

    Platamid HX 2592 F is delivered in 25 kg sealed bags and in 500 kg Big Bag. Platamid HX 2592 T is delivered in 25 kg sealed bagsThese grades are ready to be processed.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.

    RENEWABLE CARBON CONTENT 80 % (calculated, ASTM D6866)

  • This material data has been provided by Arkema Technical Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueConditionTesting Standard

    Bio-based content

    80 %

    Show Supplier Material materials with Bio-based content of 80 %

    Density

    1.09 g/cm³

    Show Supplier Material materials with Density of 1.09 g/cm³

    dry

    ISO 1183

    Thermal

    PropertyValueConditionTesting StandardComment

    Melting point

    106 °C

    Show Supplier Material materials with Melting point of 106 °C

    dry

    ISO 11357-1/-3

    10°C/min

    Rheological Properties

    PropertyValueConditionTesting StandardComment

    Melt volume-flow rate

    24 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 24 cm³/10min

    dry

    ISO 1133

    160°C/2.16kg

    Technological properties

    Property
    Application areas

    Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior