Platamid® M 1276

Alternative and trade names
PA*
Want to keep this datasheet? Save it now in your required format

Description

Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® M 1276 is a thermoplastic co-polyamide hot melt adhesive available in pellet form. This medium melt viscosity grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.

Platamid® M 1276 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, etc). In addition, Platamid® M 1276

also exhibits strong adhesion onto rigid and plasticized PVC as well as ABS, epoxy resin, PU etc. Dense layers of

Platamid® M 1276 are known to have barrier properties against PVC plasticizer migration.

This product is available:

  • Dried (M 1276 TE)
  • Un-dried (M 1276 F)

    PACKAGING

    Platamid® M 1276 TE is delivered in 25 kg sealed bags. Platamid®M 1276 F is delivered in 25 kg sealed bags and 500 kg sealed big bags (GRVS). These grades are ready to be processed.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.

    RENEWABLE CARBON: 26%

  • This material data has been provided by Arkema Technical Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueConditionTesting Standard

    Bio-based content

    26 %

    Show Supplier Material materials with Bio-based content of 26 %

    Density

    1.1 g/cm³

    Show Supplier Material materials with Density of 1.1 g/cm³

    dry

    ISO 1183

    Thermal

    PropertyValueConditionTesting StandardComment

    Melting point

    110 °C

    Show Supplier Material materials with Melting point of 110 °C

    dry

    ISO 11357-1/-3

    10°C/min

    Rheological Properties

    PropertyValueConditionTesting StandardComment

    Melt volume-flow rate

    6 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 6 cm³/10min

    dry

    ISO 1133

    160°C/2.16kg

    Technological properties

    Property
    Application areas

    Decorative Films,Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior,Hot Melt Hot Melt Adhesives Flooring - Flooring,Hot Melt Hot Melt Adhesives Interlining / Garments - Interlining / Garments,Circuit Board Adhesives