Platamid® M 1757 Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® M 1757 is a standard thermoplastic co-polyamide hot melt adhesive available in pellet form. This low to medium melt viscosity, fast re-crystallizing grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.

Platamid® M 1757 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, etc).

Platamid® M 1757 has a very good dry cleaning resistance and washing resistance up to 60°C.

This product is available:

  • Dried with optical brightener (M 1757 TA)
  • Un-dried with optical brightener (M 1757 FA)

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Thermal

    PropertyValueComment

    Melting point

    106 °C

    Show Supplier Material materials with Melting point of 106 °C

    ISO 11357-1/-3, 10°C/min

    Rheological Properties

    PropertyValueComment

    Melt volume-flow rate

    27 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 27 cm³/10min

    ISO 1133, 160°C/2.16kg

    Technological properties

    Property
    Application areas

    Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior,Hot Melt Hot Melt Adhesives Interlining / Garments - Interlining / Garments,Footwear - Uppers,Accessories

    Other

    PACKAGING

    Platamid® M 1757 TA is delivered in 25 kg sealed bags. Platamid®M 1757 FA is delivered in 500 kg sealed big bags (GRVS). These grades are ready to be processed.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.