Description

Platamid® M 2468 Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® M 2468 is a standard thermoplastic copolyamide hot melt adhesive available in pellet form. This low to medium melt viscosity grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.

Platamid® M 2468 offers a good adhesion at low fusing conditions to various polar substrates (thermoplastics, thermosets, metal, natural fibers, etc).

Platamid® M 2468 has good dry cleaning resistance and washing resistance up to 60°C.

This product is available:

  • Dried with optical brightener (M 2468 TA)
  • Un-dried with optical brightener (M 2468 FA)

    RENEWABLE CARBON CONTENT 25%

    (calculated, ASTM D6866)

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Bio-based content

    25 %

    Show Supplier Material materials with Bio-based content of 25 %

    ASTM D6866

    Density

    23.0 °C

    1.06 g/cm³

    Show Supplier Material materials with Density of 1.06 g/cm³

    ISO 1183

    Thermal

    PropertyValueComment

    Melting point

    102 °C

    Show Supplier Material materials with Melting point of 102 °C

    ISO 11357-1/-3, 10°C/min

    Rheological Properties

    PropertyValueComment

    Melt volume-flow rate

    26 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 26 cm³/10min

    ISO 1133, 160°C/2.16kg

    Technological properties

    Property
    Application areas

    Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior

    Other

    PACKAGING

    Platamid®M 2468 TA is delivered in 25 kg sealed bags and 500kg sealed big bags (GRVS). Platamid® M 2468 FA is delivered in 500kg sealed rigid containers (GRVC) and 500kg sealed big bags (GRVS). These grades are ready to be processed.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.