Rilsamid® AECHVO

Alternative and trade names
PA12
Want to keep this datasheet? Save it now in your required format

Description

PA12, KHL, 18-010

Rilsamid® AECHVO resin is a natural polyamide 12. This grade is designed for cable coating but is also suitable for extrusion.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.01 g/cm³

Show Supplier Material materials with Density of 1.01 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.2 GPa

Show Supplier Material materials with Elastic modulus of 1.2 GPa

ISO 527-1/-2, Conditioned

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal, Conditioned

Elongation at yield

23.0 °C

6 %

Show Supplier Material materials with Elongation at yield of 6 %

ISO 527-1/-2, Conditioned

Hardness, Shore D

23.0 °C

73 [-]

Show Supplier Material materials with Hardness, Shore D of 73 [-]

ISO 7619-1, 15 seconds

Yield strength

23.0 °C

38 MPa

Show Supplier Material materials with Yield strength of 38 MPa

ISO 527-1/-2, Conditioned

Thermal

PropertyValueComment

Melting point

178 °C

Show Supplier Material materials with Melting point of 178 °C

ISO 11357-1/-3, 10°C/min

Rheological Properties

PropertyValueComment

Melt volume-flow rate

45 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 45 cm³/10min

ISO 1133, 235°C/5kg

Technological properties

Property
Application areas

Main applications:

  • Wire Sheathing

    or

    Wire and Cables

  • Other

    Packaging:

  • This grade is delivered dried in sealed packaging (800 kg rigid containers) ready to be processed.

    Shelf life: Two years from date of delivery. For any used above this limit, please refer to our technical services.

  • Processing methods

    Injection Molding:

  • Extrusion temperature- Typical melt temperature (Min / Recommended / Max) : 240°C / 250°C / 260°C.
  • Drying time and temperature (only necessary for containers opened for more than two hours) : 4-8 hours at 80°C.


    Extrusion:

  • Typical melt temperature: (Min / Recommended / Max): 240°C / 250°C / 260°C
  • Drying time and temperature (only necessary if containers opened for more than two hours): 4 - 6 hours at 80°C