Rilsamid® AECV BLACK T8L

Alternative and trade names
PA12
Want to keep this datasheet? Save it now in your required format

Description

PA12, KHL, 16-010

Rilsamid® AECV BLACK T8L resin is a black colored polyamide 12. This grade is designed for cable coating.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.01 g/cm³

Show Supplier Material materials with Density of 1.01 g/cm³

ISO 1183

Water absorption

23.0 °C

1.6 %

Show Supplier Material materials with Water absorption of 1.6 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.35 GPa

Show Supplier Material materials with Elastic modulus of 1.35 GPa

ISO 527-1/-2

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal

Elongation at yield

23.0 °C

5 %

Show Supplier Material materials with Elongation at yield of 5 %

ISO 527-1/-2

Puncture energy

-30.0 °C

70 J

Show Supplier Material materials with Puncture energy of 70 J

ISO 6603-2, Conditioned

Puncture force

-30.0 °C

5000 N

Show Supplier Material materials with Puncture force of 5000 N

ISO 6603-2, Conditioned

Yield strength

23.0 °C

41 MPa

Show Supplier Material materials with Yield strength of 41 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

135 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

55 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 55 °C

ISO 75-1/-2

Melting point

178 °C

Show Supplier Material materials with Melting point of 178 °C

ISO 11357-1/-3, 10°C/min

Vicat softening temperature

138 °C

Show Supplier Material materials with Vicat softening temperature of 138 °C

ISO 306, 50°C/h 50N

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112, Conditioned

Dielectric constant, 100Hz

23.0 °C

4 [-]

Show Supplier Material materials with Dielectric constant, 100Hz of 4 [-]

IEC 60250

Dielectric constant, 1MHz

23.0 °C

3 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 3 [-]

IEC 60250

Dielectric strength

23.0 °C

40 kV/mm

Show Supplier Material materials with Dielectric strength of 40 kV/mm

IEC 60243-1, Conditioned

Dissipation factor, 100Hz

23.0 °C

0.04 [-]

Show Supplier Material materials with Dissipation factor, 100Hz of 0.04 [-]

IEC 60250

Dissipation factor, 1MHz

23.0 °C

0.02 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 [-]

IEC 60250

Rheological Properties

PropertyValueComment

Melt volume-flow rate

12 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 12 cm³/10min

ISO 1133, 235°C/2.16kg

Technological properties

Property
Application areas

Antitermite Cables,Performance Wire

Processing methods

Injection Molding:

  • Melt temperature (°C) ISO 294: 270
  • Mold temperature (°C) ISO 10724: 50
  • Injection velocity (mm/s) ISO 294: -
  • Pressure at hold (MPa) ISO 294: 16