Rilsamid® AESN BLACK P202 CTL

Alternative and trade names
PA12-I-CD
Want to keep this datasheet? Save it now in your required format

Description

PA12, EHLZ, 22-005

Rilsamid® AESN BLACK P202 CTL resin is a plasticized conductive grade designed for tube extrusion.

Rilsamid® AESN BLACK P202 CTL resin is specially designed for conductive multi-layers fuel line applications.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.585 GPa

Show Supplier Material materials with Elastic modulus of 0.585 GPa

dry

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-1/-2

min. | nominal

Elongation at yield

26 %

Show Supplier Material materials with Elongation at yield of 26 %

dry

ISO 527-1/-2

Hardness, Shore D

65 [-]

Show Supplier Material materials with Hardness, Shore D of 65 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy notched

-30 °C

4 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m²

dry

ISO 179/1eA

23 °C

82 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 82 kJ/m²

dry

ISO 179/1eA

Impact strength, Charpy unnotched

No Break at 23 and -30°C

dry

ISO 179/1eU

Yield strength

28 MPa

Show Supplier Material materials with Yield strength of 28 MPa

cond.

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Melting point

174 °C

Show Supplier Material materials with Melting point of 174 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

1.2 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 1.2 cm³/10min

dry

ISO 1133

235°C/5kg

Technological properties

Property
Application areas

Fuel Management - Fuel Lines,Tubing and Hoses