Rilsamid® AESN BLACK P302 TL

Alternative and trade names
PA12-I
Want to keep this datasheet? Save it now in your required format

Description

PA12-HIP, EHL, 22-004

Rilsamid® AESN BLACK P302 TL resin is a black colored polyamide 12. This grade is plasticized and designed for tube extrusion.

Rilsamid® AESN BLACK P302 TL resin falls into the PA12-HIPHL category according to DIN 73378.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.03 g/cm³

Show Supplier Material materials with Density of 1.03 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal, Conditioned

Elongation at yield

23.0 °C

26 %

Show Supplier Material materials with Elongation at yield of 26 %

ISO 527-1/-2, Conditioned

Yield strength

23.0 °C

25 MPa

Show Supplier Material materials with Yield strength of 25 MPa

ISO 527-1/-2, Conditioned

Thermal

PropertyValueComment

Melting point

172 °C

Show Supplier Material materials with Melting point of 172 °C

ISO 11357-1/-3, 10°C/min

Rheological Properties

PropertyValueComment

Melt volume-flow rate

18 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 18 cm³/10min

ISO 1133, 235°C/5kg

Technological properties

Property
Application areas

Air Brake Tubing,Auto - Water Cooling Circuit,Fuel Management - Fuel Lines,Pneumatic Tubing

Processing methods

Injection Molding:

  • Melt temperature (°C) ISO 294: 270
  • Mold temperature (°C) ISO 10724: 50
  • Injection velocity (mm/s) ISO 294: -
  • Pressure at hold (MPa) ISO 294: 16