Rilsamid® AESN BLACK P401 TL

Alternative and trade names
PA12
Want to keep this datasheet? Save it now in your required format

Description

Rilsamid® AESN BLACK P401 TL resin is a black colored polyamide. This grade is plasticized and designed for tube extrusion.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.03 g/cm³

Show Supplier Material materials with Density of 1.03 g/cm³

dry

ISO 1183

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.332 GPa

Show Supplier Material materials with Elastic modulus of 0.332 GPa

cond.

ISO 527-1/-2

0.34 GPa

Show Supplier Material materials with Elastic modulus of 0.34 GPa

dry

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min.

Hardness, Shore D

61 [-]

Show Supplier Material materials with Hardness, Shore D of 61 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy notched

-30 °C

2.4 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 2.4 kJ/m²

dry

ISO 179/1eA

No Break at 23°C

-30 °C

7 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m²

cond.

ISO 179/1eA

No Break at 23°C

Impact strength, Charpy unnotched

No Break at 23 and -30°C

dry and cond.

ISO 179/1eU

Yield strength

44 MPa

Show Supplier Material materials with Yield strength of 44 MPa

cond.

ISO 527-1/-2

50 MPa

Show Supplier Material materials with Yield strength of 50 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Melting point

180 °C

Show Supplier Material materials with Melting point of 180 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

8 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 8 cm³/10min

dry

ISO 1133

235°C/2.16kg

Technological properties

Property
Application areas

Air Brake Tubing,Fuel Management - Fuel Lines