Description

Rilsamid® AESNO MED is a rigid polyamide 12 with high viscosity designed for tube extrusion. This grade, dedicated to extrusion, offers the highest quality and it is specifically designed to meet the stringent requirements of the medical applications such as minimally invasive devices. Upon request letters regarding USP Class VI compliance can be provided.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.01 g/cm³

Show Supplier Material materials with Density of 1.01 g/cm³

ISO 1183

Water absorption

23.0 °C

1.6 %

Show Supplier Material materials with Water absorption of 1.6 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.5 GPa

Show Supplier Material materials with Elastic modulus of 1.5 GPa

ISO 527-1/-2

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal

Elongation at yield

23.0 °C

5 %

Show Supplier Material materials with Elongation at yield of 5 %

ISO 527-1/-2

Puncture energy

-30.0 °C

60 J

Show Supplier Material materials with Puncture energy of 60 J

ISO 6603-2, Conditioned

Puncture force

-30.0 °C

4800 N

Show Supplier Material materials with Puncture force of 4800 N

ISO 6603-2, Conditioned

Yield strength

23.0 °C

50 MPa

Show Supplier Material materials with Yield strength of 50 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

135 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

55 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 55 °C

ISO 75-1/-2

Melting point

180 °C

Show Supplier Material materials with Melting point of 180 °C

ISO 11357-1/-3, 10°C/min

Vicat softening temperature

142 °C

Show Supplier Material materials with Vicat softening temperature of 142 °C

ISO 306, 50°C/h 50N

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112, Conditioned

Dielectric strength

23.0 °C

30 kV/mm

Show Supplier Material materials with Dielectric strength of 30 kV/mm

IEC 60243-1, Conditioned

Rheological Properties

PropertyValueComment

Melt volume-flow rate

8 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 8 cm³/10min

ISO 1133, 235°C/5kg

Technological properties

Property
Application areas

Tubing and Hoses,Healthcare-Other,Medical Catheters

Certifications

USP Class VI