Description

Rilsamid® AESNO P10 TL resin is a plasticized conductive grade designed for tube extrusion. AESNO P10 TL resin is a natural polyamide 12. This grade is plasticized and designed for tube extrusion.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.03 g/cm³

Show Supplier Material materials with Density of 1.03 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.71 GPa

Show Supplier Material materials with Elastic modulus of 0.71 GPa

ISO 527-1/-2, Conditioned

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal, Conditioned

Elongation at yield

23.0 °C

20 %

Show Supplier Material materials with Elongation at yield of 20 %

ISO 527-1/-2, Conditioned

Hardness, Shore D

23.0 °C

69 [-]

Show Supplier Material materials with Hardness, Shore D of 69 [-]

ISO 7619-1, 15 seconds

Thermal

PropertyValueComment

Melting point

180 °C

Show Supplier Material materials with Melting point of 180 °C

ISO 11357-1/-3, 10°C/min

Rheological Properties

PropertyValueComment

Melt volume-flow rate

8 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 8 cm³/10min

ISO 1133, 235°C/2.16kg