Rilsamid® AMN BLACK P40 TLD

Alternative and trade names
PA12
Want to keep this datasheet? Save it now in your required format

Description

PA12-P, MHLR, 12-004

Rilsamid® AMN BLACK P40 TLD resin is a black colored polyamide. This black grade is plasticized and designed for injection molding.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

dry

ISO 1183

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.46 GPa

Show Supplier Material materials with Elastic modulus of 0.46 GPa

cond.

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min. | nominal

Elongation at yield

26 %

Show Supplier Material materials with Elongation at yield of 26 %

cond.

ISO 527-1/-2

Impact strength, Charpy notched

-30 °C

4 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m²

cond.

ISO 179/1eA

23 °C

25 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m²

cond.

ISO 179/1eA

Impact strength, Charpy unnotched

No Break at 23 and -30°C

cond.

ISO 179/1eU

Yield strength

46 MPa

Show Supplier Material materials with Yield strength of 46 MPa

cond.

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Melting point

172 °C

Show Supplier Material materials with Melting point of 172 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

51 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 51 cm³/10min

dry

ISO 1133

235°C/2.16kg

Shrinkage

1 %

Show Supplier Material materials with Shrinkage of 1 %

dry

ISO 294-4

1.3 %

Show Supplier Material materials with Shrinkage of 1.3 %

dry

ISO 294-4

Transverse

Technological properties

Property
Application areas

Chemical Process Industry - Injection Molding

Processing methods

Injection Molding:

  • Melt temperature (°C) ISO 294: 250
  • Mold temperature (°C) ISO 10724: 40
  • Injection velocity (mm/s) ISO 294: -
  • Pressure at hold (MPa) ISO 294: 16