Description

Rilsamid® AMNO MED is a thermoplastic polyamide 12. This grade dedicated to injection offers highest quality and it is specifically designed to meet the stringent requirements of the medical applications such as minimally invasive devices. Upon request letters regarding USP Class VI compliance can be provided.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.01 g/cm³

Show Supplier Material materials with Density of 1.01 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal, Conditioned

Elongation at yield

23.0 °C

8 %

Show Supplier Material materials with Elongation at yield of 8 %

ISO 527-1/-2, Conditioned

Thermal

PropertyValueComment

Melting point

180 °C

Show Supplier Material materials with Melting point of 180 °C

ISO 11357-1/-3, 10°C/min

Rheological Properties

PropertyValueComment

Melt volume-flow rate

57 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 57 cm³/10min

ISO 1133, 235°C/2.16kg

Technological properties

Property
Application areas

Healthcare-Other,Medical Catheters

Certifications

USP Class VI

Processing methods

Injection Molding:

  • Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.
  • Mold temperature : 40°C
  • Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 60-80°C.