Rilsamid® AZM 23 BLACK T6LD

Alternative and trade names
PA12-GF23
Want to keep this datasheet? Save it now in your required format

Description

PA12, MHLR, 16-060, GF23

Rilsamid® AZM 23 BLACK T6LD resin is a fiberglass reinforced polyamide. This black colored grade is designed for injection moulding.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.5 %

Show Supplier Material materials with Moisture absorption of 0.5 %

Sim. to ISO 62

Water absorption

23.0 °C

1.3 %

Show Supplier Material materials with Water absorption of 1.3 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

5.5 GPa

Show Supplier Material materials with Elastic modulus of 5.5 GPa

ISO 527-1/-2

Elongation

23.0 °C

5.2 %

Show Supplier Material materials with Elongation of 5.2 %

ISO 527-1/-2, nominal, Conditioned

Elongation at yield

23.0 °C

3 %

Show Supplier Material materials with Elongation at yield of 3 %

ISO 527-1/-2

Impact strength, Charpy notched

-30.0 °C

8 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m²

ISO 179/1eA

23.0 °C

15 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

-30.0 °C

66 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 66 kJ/m²

ISO 179/1eU

23.0 °C

66 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 66 kJ/m²

ISO 179/1eU

Unlock all property charts

Tensile strength

23.0 °C

95 MPa

Show Supplier Material materials with Tensile strength of 95 MPa

ISO 527-1/-2

Yield strength

23.0 °C

101 MPa

Show Supplier Material materials with Yield strength of 101 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 6E-5 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

173 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 173 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

165 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 165 °C

ISO 75-1/-2

Melting point

179 °C

Show Supplier Material materials with Melting point of 179 °C

ISO 11357-1/-3, 10°C/min

Thermal decomposition in air

222 °C

Show Supplier Material materials with Thermal decomposition in air of 222 °C

TGA, 1% wt. loss

Thermal decomposition in nitrogen

223 °C

Show Supplier Material materials with Thermal decomposition in nitrogen of 223 °C

TGA, 1% wt. loss

Vicat softening temperature

165 °C

Show Supplier Material materials with Vicat softening temperature of 165 °C

ISO 306, 50°C/h 50N

Electrical

PropertyTemperatureValueComment

Dielectric constant, 100Hz

23.0 °C

5 [-]

Show Supplier Material materials with Dielectric constant, 100Hz of 5 [-]

IEC 60250

Dielectric constant, 1MHz

23.0 °C

5 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 5 [-]

IEC 60250

Dissipation factor, 100Hz

23.0 °C

0.12 [-]

Show Supplier Material materials with Dissipation factor, 100Hz of 0.12 [-]

IEC 60250

Dissipation factor, 1MHz

23.0 °C

0.04 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.04 [-]

IEC 60250

Rheological Properties

PropertyValueComment

Melt volume-flow rate

13 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 13 cm³/10min

ISO 1133, 235°C/5kg

Technological properties

Property
Application areas

Connectors

Fillers

23% Glass Fiber

Processing methods

Injection Molding:

  • Melt temperature (°C) ISO 294: 280
  • Mold temperature (°C) ISO 10724: 60
  • Injection velocity (mm/s) ISO 294: -
  • Pressure at hold (MPa) ISO 294: 16