Rilsamid® AZM 30 BLACK T6LD

Alternative and trade names
PA12-GF30
Want to keep this datasheet? Save it now in your required format

Description

PA12, MHLR, 16-060, GF30

Rilsamid® AZM 30 BLACK T6LD resin is a fiberglass reinforced polyamide. This black colored grade is designed for injection molding.(norme ISO 19396-1/2015)

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.24 g/cm³

Show Supplier Material materials with Density of 1.24 g/cm³

dry

ISO 1183

Moisture absorption

0.5 %

Show Supplier Material materials with Moisture absorption of 0.5 %

Sim. to ISO 62

Water absorption

1.3 %

Show Supplier Material materials with Water absorption of 1.3 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting Standard

Elastic modulus

6.4 GPa

Show Supplier Material materials with Elastic modulus of 6.4 GPa

cond.

ISO 527-1/-2

6.9 GPa

Show Supplier Material materials with Elastic modulus of 6.9 GPa

dry

ISO 527-1/-2

Elongation

4 %

Show Supplier Material materials with Elongation of 4 %

cond.

ISO 527-1/-2

5 %

Show Supplier Material materials with Elongation of 5 %

dry

ISO 527-1/-2

Elongation at yield

3 %

Show Supplier Material materials with Elongation at yield of 3 %

dry

ISO 527-1/-2

4 %

Show Supplier Material materials with Elongation at yield of 4 %

cond.

ISO 527-1/-2

Impact strength, Charpy notched

-30 °C

12 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m²

cond., dry

ISO 179/1eA

23 °C

19 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 19 kJ/m²

cond., dry

ISO 179/1eA

Impact strength, Charpy unnotched

-30 °C

83 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 83 kJ/m²

dry, cond.

ISO 179/1eU

23 °C

77 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 77 kJ/m²

cond.

ISO 179/1eU

23 °C

79 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 79 kJ/m²

dry

ISO 179/1eU

Unlock all property charts

Tensile strength

100 MPa

Show Supplier Material materials with Tensile strength of 100 MPa

cond.

ISO 527-1/-2

112 MPa

Show Supplier Material materials with Tensile strength of 112 MPa

dry

ISO 527-1/-2

Yield strength

115 MPa

Show Supplier Material materials with Yield strength of 115 MPa

cond.

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Coefficient of thermal expansion

5e-05 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5e-05 1/K

dry

ISO 11359-1/-2

Melting point

183 °C

Show Supplier Material materials with Melting point of 183 °C

dry

ISO 11357-1/-3

10°C/min

Thermal decomposition in air

227 °C

Show Supplier Material materials with Thermal decomposition in air of 227 °C

TGA

1% wt. loss

Thermal decomposition in nitrogen

224 °C

Show Supplier Material materials with Thermal decomposition in nitrogen of 224 °C

TGA

1% wt. loss

Vicat softening temperature

165 °C

Show Supplier Material materials with Vicat softening temperature of 165 °C

ISO 306

50°C/h 50N

Flammability

At thickness 3.2 mm IEC 60695-11-10: HB and yellow card available

Electrical

PropertyValueConditionTesting StandardFrequency

Comparative tracking index

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

cond.

IEC 60112

Dielectric constant

3 [-]

Show Supplier Material materials with Dielectric constant of 3 [-]

dry

IEC 60250

1MHz

4 [-]

Show Supplier Material materials with Dielectric constant of 4 [-]

dry

IEC 60250

100Hz

Dielectric strength

35 kV/mm

Show Supplier Material materials with Dielectric strength of 35 kV/mm

cond., dry

IEC 60243-1

Dissipation factor

0.0274 [-]

Show Supplier Material materials with Dissipation factor of 0.0274 [-]

dry

IEC 60250

1MHz

0.0664 [-]

Show Supplier Material materials with Dissipation factor of 0.0664 [-]

dry

IEC 60250

100Hz

Surface resistivity

1e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

cond.

IEC 60093

Volume resistivity

1e+11 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm

cond.

IEC 60093

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

7 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 7 cm³/10min

dry

ISO 1133

235°C/5kg

Technological properties

Property
Application areas

Connectors,Fittings, Components, and Injection Molded Parts

Certifications

Yellow Card

Fillers

30% Glass Fiber

Processing methods

Injection Molding:

  • Melt temperature (°C) ISO 294: 280
  • Mold temperature (°C) ISO 10724: 60
  • Injection velocity (mm/s) ISO 294: -
  • Pressure at hold (MPa) ISO 294: 16