Rilsamid® DZM 30 BLACK TL

Alternative and trade names
PA612-GF30
Want to keep this datasheet? Save it now in your required format

Description

Rilsamid® DZM 30 BLACK TL resin

  • Rilsamid® POLYAMIDE 612 (PA612)

    Rilsamid® DZM 30 BLACK TL is a stabilized Polyamide 612 resin reinforced with 30% glass fiber. This black grade is designed for injection molding application.

  • This material data has been provided by Arkema Technical Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueConditionTesting Standard

    Density

    1.28 g/cm³

    Show Supplier Material materials with Density of 1.28 g/cm³

    dry

    ISO 1183

    Moisture absorption

    0.8 %

    Show Supplier Material materials with Moisture absorption of 0.8 %

    Sim. to ISO 62

    Mechanical

    PropertyTemperatureValueConditionTesting Standard

    Elastic modulus

    7.8 GPa

    Show Supplier Material materials with Elastic modulus of 7.8 GPa

    dry

    ISO 527-1/-2

    Elongation

    5 %

    Show Supplier Material materials with Elongation of 5 %

    dry

    ISO 527-1/-2

    Impact strength, Charpy notched

    -30 °C

    13 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m²

    dry

    ISO 179/1eA

    23 °C

    20 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m²

    dry

    ISO 179/1eA

    Impact strength, Charpy unnotched

    -30 °C

    90 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

    dry

    ISO 179/1eU

    23 °C

    90 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

    dry

    ISO 179/1eU

    Unlock all property charts

    Tensile strength

    137 MPa

    Show Supplier Material materials with Tensile strength of 137 MPa

    dry

    ISO 527-1/-2

    Yield strength

    25 MPa

    Show Supplier Material materials with Yield strength of 25 MPa

    dry

    ISO 527-1/-2

    Thermal

    PropertyValueConditionTesting StandardComment

    Melting point

    215 °C

    Show Supplier Material materials with Melting point of 215 °C

    dry

    ISO 11357-1/-3

    10°C/min

    Vicat softening temperature

    210 °C

    Show Supplier Material materials with Vicat softening temperature of 210 °C

    ISO 306

    50°C/h 50N

    Rheological Properties

    PropertyValueConditionTesting StandardComment

    Shrinkage

    0.4 %

    Show Supplier Material materials with Shrinkage of 0.4 %

    dry

    ISO 294-4

    1 %

    Show Supplier Material materials with Shrinkage of 1 %

    dry

    ISO 294-4

    Transverse

    Technological properties

    Property
    Application areas

    Connectors,Fittings, Components, and Injection Molded Parts

    Fillers

    30% Glass Fiber