Rilsamid® MA 4411 BLACK

Alternative and trade names
PA12-I
Want to keep this datasheet? Save it now in your required format

Description

PA12, MHLR, 16-010

Rilsamid® MA 4411 BLACK resin is plasticized and designed for tube extrusion.

Rilsamid® MA 4411 BLACK resin falls into the PA12-HIPHL category according to DIN 73378 (PA12-HIP, EHL, 22-004).

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.03 g/cm³

Show Supplier Material materials with Density of 1.03 g/cm³

dry

ISO 1183

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.47 GPa

Show Supplier Material materials with Elastic modulus of 0.47 GPa

dry

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-1/-2

min. | nominal

Elongation at yield

23 %

Show Supplier Material materials with Elongation at yield of 23 %

dry

ISO 527-1/-2

Hardness, Shore D

63 [-]

Show Supplier Material materials with Hardness, Shore D of 63 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy notched

-30 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

dry

ISO 179/1eA

No Break at 23°C

Impact strength, Charpy unnotched

No Break at 23 and -30°C

dry

ISO 179/1eU

Thermal

PropertyValueConditionTesting StandardComment

Melting point

175 °C

Show Supplier Material materials with Melting point of 175 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

14 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 14 cm³/10min

dry

ISO 1133

235°C/5kg

Technological properties

Property
Application areas

Tubing and Hoses