Rilsamid® MA 4411 NAT

Alternative and trade names
PA12-I
Want to keep this datasheet? Save it now in your required format

Description

PA12, MHLR, 16-010

Rilsamid® MA 4411 NAT resin is a natural polyamide. This grade is plasticized and designed for tube extrusion.

Rilsamid® MA 4411 NAT resin falls into the PA12-HIPHL category according to DIN 73378 (PA12-HIP, EHL, 22-004). This grade is also available in black.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.03 g/cm³

Show Supplier Material materials with Density of 1.03 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.47 GPa

Show Supplier Material materials with Elastic modulus of 0.47 GPa

ISO 527-1/-2

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal

Elongation at yield

23.0 °C

23 %

Show Supplier Material materials with Elongation at yield of 23 %

ISO 527-1/-2

Hardness, Shore D

23.0 °C

63 [-]

Show Supplier Material materials with Hardness, Shore D of 63 [-]

ISO 7619-1, 15 seconds

Impact strength, Charpy notched

-30.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

No break @ 23°C, ISO 179/1eA

Yield strength

23.0 °C

25 MPa

Show Supplier Material materials with Yield strength of 25 MPa

ISO 527-1/-2

Impact strength, Charpy unnotched

No break @ 23,-30°C, ISO 179/1eU

Thermal

PropertyValueComment

Melting point

175 °C

Show Supplier Material materials with Melting point of 175 °C

ISO 11357-1/-3, 10°C/min

Rheological Properties

PropertyValueComment

Melt volume-flow rate

14 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 14 cm³/10min

ISO 1133, 235°C/5kg

Technological properties

Property
Application areas

Tubing and Hoses