Rilsan® BESN BLACK P212 CTL

Alternative and trade names
PA11-I-CD
Want to keep this datasheet? Save it now in your required format

Description

PA11-P, EHL, 22-007-CD22

Rilsan® PA 11 G BESN BLACK P212 CTL resin is a polyamide 11 produced from a renewable source. This black grade is specially designed for conductive multi-layers fuel line applications. The percentage of renewable carbon according to ASTM D6866 (calculated) is 55%.

Packaging:

This grade is delivered dried in sealed packaging (44 lb bags) ready to be processed.

Shelf Life:

Two years from the delivery. For any use above this limit, please refer to our technical services.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Bio-based content

55 %

Show Supplier Material materials with Bio-based content of 55 %

Density

1.16 g/cm³

Show Supplier Material materials with Density of 1.16 g/cm³

dry

ISO 1183

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.705 GPa

Show Supplier Material materials with Elastic modulus of 0.705 GPa

cond.

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min. | nominal

Elongation at yield

45 %

Show Supplier Material materials with Elongation at yield of 45 %

cond.

ISO 527-1/-2

Hardness, Shore D

66 [-]

Show Supplier Material materials with Hardness, Shore D of 66 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy notched

-30 °C

9 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m²

cond.

ISO 179/1eA

No Break at 23°C

Impact strength, Charpy unnotched

No Break at 23 and -30°C

cond.

ISO 179/1eU

Yield strength

27 MPa

Show Supplier Material materials with Yield strength of 27 MPa

cond.

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Melting point

182 °C

Show Supplier Material materials with Melting point of 182 °C

dry

ISO 11357-1/-3

10°C/min

Technological properties

Property
Application areas

Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines

Fillers

Carbon Black

Processing methods

Extrusion:

  • Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.
  • Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.