Rilsan® BESNO 400 TL NL

Alternative and trade names
PA11
Want to keep this datasheet? Save it now in your required format

Description

PA11-HIP, EHL, 22-0052

Rilsan® BESNO P400 TL NL resin is a polyamide 11 produced from a renewable source. This natural grade is plasticized and designed for extrusion.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1 g/cm³

Show Supplier Material materials with Density of 1 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.19 GPa

Show Supplier Material materials with Elastic modulus of 0.19 GPa

ISO 527-1/-2, Conditioned

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal, Conditioned

Hardness, Shore D

23.0 °C

49 [-]

Show Supplier Material materials with Hardness, Shore D of 49 [-]

ISO 7619-1, 15 seconds

Tensile strength

23.0 °C

36 MPa

Show Supplier Material materials with Tensile strength of 36 MPa

ISO 527-1/-2, Conditioned

Thermal

PropertyValueComment

Melting point

182 °C

Show Supplier Material materials with Melting point of 182 °C

ISO 11357-1/-3, 10°C/min

Technological properties

Property
Application areas

Main applications: Fluid transportation, Offshore Flexible Pipes

Other

Packaging:

  • This grade is delivered dried in sealed packaging (550 kg rigid containers)) ready to be processed.

    Shelf Life:Two years from the delivery. For any use above this limit, please refer to our technical services.