Rilsan® BESNO MED

Alternative and trade names
PA11
Want to keep this datasheet? Save it now in your required format

Description

PA11,EHL,22-010

Rilsan® BESNO MED resin is a polyamide 11 produced from a renewable source. This grade dedicated to extrusion offers the highest quality and it is specifically designed to meet the stringent requirements of the medical applications such as minimally invasive devices. Upon request, letters regarding USP Class VI compliance can be provided. The percentage of renewable carbon according to ASTM D6866 (calculated) is 100%.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Bio-based content

100 %

Show Supplier Material materials with Bio-based content of 100 %

Density

1.02 g/cm³

Show Supplier Material materials with Density of 1.02 g/cm³

dry

ISO 1183

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

1.2 GPa

Show Supplier Material materials with Elastic modulus of 1.2 GPa

cond.

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min. | nominal

Elongation at yield

6 %

Show Supplier Material materials with Elongation at yield of 6 %

cond.

ISO 527-1/-2

Hardness, Shore D

71 [-]

Show Supplier Material materials with Hardness, Shore D of 71 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy notched

-30 °C

13 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m²

cond.

ISO 179/1eA

23 °C

15 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m²

cond.

ISO 179/1eA

Impact strength, Charpy unnotched

No Break at 23 and -30°C

cond.

ISO 179/1eU

Yield strength

31 MPa

Show Supplier Material materials with Yield strength of 31 MPa

cond.

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Melting point

186 °C

Show Supplier Material materials with Melting point of 186 °C

dry

ISO 11357-1/-3

10°C/min

Technological properties

Property
Application areas

Wire and Cables,Healthcare-Other,IV Bags,Medical Catheters

Certifications

USP Class VI

Processing methods

Extrusion:

  • Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.
  • Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 65-80°C.