Rilsan® BESNO P40 TLX NL

Alternative and trade names
PA11
Want to keep this datasheet? Save it now in your required format

Description

PA11-P, EHL, 22-003

Rilsan® BESNO P40 TLX NL resin is a polyamide 11 produced from a renewable source. This natural grade is plasticized and designed for extrusion of large pipe as used in Oil and Gaz applications. This grade does not contain any lubricant. The percentage of renewable carbon according to ASTM D6866 (calculated) is 89%.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Bio-based content

89 %

Show Supplier Material materials with Bio-based content of 89 %

Density

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

dry

ISO 1183

Water absorption

1.6 %

Show Supplier Material materials with Water absorption of 1.6 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.345 GPa

Show Supplier Material materials with Elastic modulus of 0.345 GPa

cond.

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min. | nominal

Elongation at yield

50 %

Show Supplier Material materials with Elongation at yield of 50 %

cond.

ISO 527-1/-2

Hardness, Shore D

60 [-]

Show Supplier Material materials with Hardness, Shore D of 60 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy notched

-30 °C

7 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m²

cond.

ISO 179/1eA

No Break at 23°C

Impact strength, Charpy unnotched

No Break at 23 and -30°C

cond.

ISO 179/1eU

Yield strength

24 MPa

Show Supplier Material materials with Yield strength of 24 MPa

cond.

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Melting point

181 °C

Show Supplier Material materials with Melting point of 181 °C

dry

ISO 11357-1/-3

10°C/min

Technological properties

Property
Application areas

Main applications:

  • Fluid transportation for Oil and Gaz sector

    Packaging: This grade is delivered dried in sealed packaging (550 kg rigid containers, 1000 lb rigid containers) ready to be processed.

    Shelf life: Two years from the delivery. For any use above this limit, please refer to our technical services.

  • Processing methods

    Extrusion:

  • Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.
  • Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.