Rilsan® BLACK RDP 15-10 FB

Alternative and trade names
PA11, Approximate RAL number: 9010
Want to keep this datasheet? Save it now in your required format

Description

Rilsan® Black Fluid Bed Powder

Rilsan® fluid bed powders are thermoplastic polyamides obtained from renewable resources. Outstanding characteristics: abrasion resistance, corrosion resistance, impact resistance, sound reduction, flexibility, low coefficient of friction.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Abrasion resistance, weight loss

16 mg

Show Supplier Material materials with Abrasion resistance, weight loss of 16 mg

ASTM D1044, Wheel CS 17, load 1 kg, 1000 cycles

Relative density

23.0 °C

1.12 [-]

Show Supplier Material materials with Relative density of 1.12 [-]

ISO 1183

Mechanical

PropertyTemperatureValueComment

Impact energy, coating

23.0 °C

160 J

Show Supplier Material materials with Impact energy, coating of 160 J

ASTM D2794

Thermal

PropertyValueComment

Melting point

183 - 193 °C

Show Supplier Material materials with Melting point of 183 - 193 °C

ISO 1218

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

200 kV/mm

Show Supplier Material materials with Dielectric strength of 200 kV/mm

ASTM D149, thickness = 150mm

Technological properties

Property
Application areas

Main applications:

  • Coating of wire goods and piping components exposed to high weathering or corrosive environments
  • Coating of machinery exposed to high abrasion such as spline shafts
  • Coating of springs for sound reduction
  • Rilsan® fluid bed powders are designed to coat metal substrates via fluidized powder bed dipping
  • Powder Coatings - Automotive & Transportation and Mining

  • Color

    Black

    Covering efficiency

    0.34 kg/m²

    Covering efficiency, thickness

    300 µm

    Other

    Additional info:

  • Smooth texture with a glossy appearance
  • Good adhesion after over 2000 hours of salt spray testing (ISO 9227)
  • Only 15% fine particles < 75 µm (ASTM D3451)
  • Only 1% coarse particles > 212 µm (ASTM D3451)
  • Only 0.1% coarse particles > 250 µm (ASTM D3451)
  • 5 year shelf life from date of delivery
  • Available in 100 lb drums