Rilsan® D30 NATURAL

Alternative and trade names
PA11
Want to keep this datasheet? Save it now in your required format

Description

RILSAN® D30 NAT is a polyamide 11 powder obtained from renewable resources with an average diameter of 21-27 µm.

RILSAN® D is a range of high performance fine polyamide powders used as multifunctional additives in coatings and varnishes.

The introduction of RILSAN® polyamide powders in formulations is easy thanks to their good dispersion capacity, their reduced Impact on rheology and their low density.

RILSAN® polyamide powders are surface modifiers, specifically designed for texture creation.

Abrasion, scratch, impact resistances and flexibility of coatings, inks and varnishes can be significantly improved using RILSAN® polyamide powders.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTesting StandardComment

Density

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

ISO 1183

relative density

Median particles size

21 - 27 μm

Show Supplier Material materials with Median particles size of 21 - 27 μm

ISO 13320

Non Tap density

0.34 g/cm³

Show Supplier Material materials with Non Tap density of 0.34 g/cm³

ISO 1068

Water absorption

1 %

Show Supplier Material materials with Water absorption of 1 %

ISO 62-1

max. | for 24h

Thermal

PropertyValueConditionTesting Standard

Melting point

186 °C

Show Supplier Material materials with Melting point of 186 °C

dry

ISO 1218

Technological properties

Property
Application areas

Main applications:

  • Coil coating
  • Wood coating
  • Plastic coating

    Packaging: This grade is delivered in 20kg bag.

    Shelf Life** Five years from the date of delivery. For any use after this limit, please refer to our technical services.