Description

RILSAN® D40 NAT is a polyamide 11 powder obtained from renewable resources with an average diameter of 27-31 µm.

RILSAN® D is a range of high performance fine polyamide powders used as multifunctional additives in coatings and varnishes.

The introduction of RILSAN® polyamide powders in formulations is easy thanks to their good dispersion capacity, their reduced Impact on rheology and their low density.

RILSAN® polyamide powders are surface modifiers, specifically designed for texture creation.

Abrasion, scratch, impact resistances and flexibility of coatings, inks and varnishes can be significantly improved using RILSAN® polyamide powders.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTesting StandardComment

Density

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

ISO 1183

relative density

Median particles size

27 - 31 μm

Show Supplier Material materials with Median particles size of 27 - 31 μm

ISO 13320

Non Tap density

0.37 g/cm³

Show Supplier Material materials with Non Tap density of 0.37 g/cm³

ISO 1068

Water absorption

1.9 %

Show Supplier Material materials with Water absorption of 1.9 %

Sim. to ISO 62

Thermal

PropertyValueConditionTesting StandardComment

Melting point

185 °C

Show Supplier Material materials with Melting point of 185 °C

dry

ISO 11357-1/-3

10°C/min

Vicat softening temperature

160 °C

Show Supplier Material materials with Vicat softening temperature of 160 °C

ISO 306

50°C/h 50N

Flammability

At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: V-2

Electrical

PropertyValueConditionTesting Standard

Dielectric strength

30 kV/mm

Show Supplier Material materials with Dielectric strength of 30 kV/mm

dry

IEC 60243-1

Surface resistivity

1e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

cond.

IEC 60093

Volume resistivity

1e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm

dry

IEC 60093

Technological properties

Property
Application areas

Main applications:

  • Coil coating
  • Wood coating
  • Plastic coating

    Packaging: This grade is delivered in 20kg bag.

    Shelf Life** Five years from the date of delivery. For any use after this limit, please refer to our technical services.