Rilsan® ESY BLACK 7260

Alternative and trade names
PA11
Want to keep this datasheet? Save it now in your required format

Description

Powder ESY BLACK 7260

  • Rilsan® POLYAMIDE 11 (PA11) Powder

    Melt mix black powder for coating of metallic parts by electrostatic spray, and post fused in an oven. There is a wide range of colors. The properties listed in the data base have been measured on a corresponding Rilsan® PA11 Granule.

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Abrasion resistance, weight loss

    17 mg

    Show Supplier Material materials with Abrasion resistance, weight loss of 17 mg

    ISO 9352, Wheel CS 17, load 1 kg, 1000 cycles

    Density

    23.0 °C

    1.35 g/cm³

    Show Supplier Material materials with Density of 1.35 g/cm³

    ISO 1183

    Median particles size

    30 μm

    Show Supplier Material materials with Median particles size of 30 μm

    ISO 13320

    Non Tap density

    23.0 °C

    0.43 g/cm³

    Show Supplier Material materials with Non Tap density of 0.43 g/cm³

    ISO 1068

    Relative density

    23.0 °C

    1.35 [-]

    Show Supplier Material materials with Relative density of 1.35 [-]

    ISO 1183

    Tap density

    23.0 °C

    0.63 g/cm³

    Show Supplier Material materials with Tap density of 0.63 g/cm³

    ISO 1068

    Water absorption

    23.0 °C

    1.9 %

    Show Supplier Material materials with Water absorption of 1.9 %

    Sim. to ISO 62

    Mechanical

    PropertyValueComment

    Hardness, Persoz

    270 [-]

    Show Supplier Material materials with Hardness, Persoz of 270 [-]

    ISO 1522

    Hardness, Pencil test

    ECCA T4: B

    Thermal

    PropertyValueComment

    Melting point

    185 °C

    Show Supplier Material materials with Melting point of 185 °C

    ISO 11357-1/-3, 10°C/min

    Vicat softening temperature

    160 °C

    Show Supplier Material materials with Vicat softening temperature of 160 °C

    ISO 306, 50°C/h 50N

    Flammability

    At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: V-2

    Electrical

    PropertyTemperatureValueComment

    Dielectric strength

    23.0 °C

    30 kV/mm

    Show Supplier Material materials with Dielectric strength of 30 kV/mm

    IEC 60243-1

    Volume resistivity

    23.0 °C

    1.00E+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm

    IEC 60093

    Technological properties

    Property
    Color

    Black

    Covering efficiency

    0.2 kg/m²

    Covering efficiency, thickness

    100 µm