Rilsan® NATURAL RDP 15-10 ES

Alternative and trade names
PA11
Want to keep this datasheet? Save it now in your required format

Description

Rilsan® Natural Electrostatic Spray Powder Rilsan® electrostatic spray powders are thermoplastic polyamides obtained from renewable resources. Outstanding characteristics: abrasion resistance, corrosion resistance, impact resistance, sound reduction, flexibility, low coefficient of friction.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTesting StandardComment

Density

1.11 g/cm³

Show Supplier Material materials with Density of 1.11 g/cm³

ISO 1183

relative density

Mechanical

PropertyValueTesting Standard

Impact energy, coating

160 J

Show Supplier Material materials with Impact energy, coating of 160 J

ASTM D2794

Thermal

PropertyValueConditionTesting Standard

Melting point

183 - 188 °C

Show Supplier Material materials with Melting point of 183 - 188 °C

dry

ISO 1218

Electrical

PropertyValueTesting StandardComment

Dielectric strength

1700 kV/mm

Show Supplier Material materials with Dielectric strength of 1700 kV/mm

ASTM D149

thickness = 150mm

Technological properties

Property
Application areas

Powder Coatings - Automotive & Transportation,Powder Coatings - General Purpose

Color

Natural

Covering efficiency

0.14 kg/m²

Covering efficiency, thickness

120 µm