Rilsan® SESHVO

Alternative and trade names
PA610
Want to keep this datasheet? Save it now in your required format

Description

Rilsan® SESHVO resin

  • Rilsan® POLYAMIDE 610 (PA610)

    Rilsan® SESHVO resin is a dried polyamide 610 neat resin produced partially from a renewable source. This natural grade is a designed for compounding and extrusion. Percentage of renewable carbon according to ASTM D6866: 60%.

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Bio-based content

    60 %

    Show Supplier Material materials with Bio-based content of 60 %

    ASTM D6866

    Density

    23.0 °C

    1.08 g/cm³

    Show Supplier Material materials with Density of 1.08 g/cm³

    ISO 1183

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    2 GPa

    Show Supplier Material materials with Elastic modulus of 2 GPa

    ISO 527-1/-2

    Impact strength, Charpy notched

    -30.0 °C

    7 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m²

    23.0 °C

    8 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m²

    Impact strength, Charpy unnotched

    No break @ 23,-30°C, ISO 179/1eU

    Thermal

    PropertyValueComment

    Heat deflection temperature, 1.80 MPa

    60 °C

    Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 60 °C

    ISO 75-1/-2

    Melting point

    222 °C

    Show Supplier Material materials with Melting point of 222 °C