Rilsan® SMNO F

Alternative and trade names
PA610
Want to keep this datasheet? Save it now in your required format

Description

Rilsan® SMNO F resin

  • Rilsan® POLYAMIDE 610 (PA610)

    Rilsan® SMNO F is an undried polyamide 610 resin produced partially from a renewable source. This natural grade is designed for compounding applications. Percentage of renewable carbon according to ASTM D6866: 60%.

  • This material data has been provided by Arkema Technical Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueConditionTesting Standard

    Bio-based content

    60 %

    Show Supplier Material materials with Bio-based content of 60 %

    Density

    1.08 g/cm³

    Show Supplier Material materials with Density of 1.08 g/cm³

    dry

    ISO 1183

    Mechanical

    PropertyTemperatureValueConditionTesting Standard

    Elastic modulus

    1.7 GPa

    Show Supplier Material materials with Elastic modulus of 1.7 GPa

    dry

    ISO 527-1/-2

    Impact strength, Charpy notched

    -30 °C

    5 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m²

    dry

    ISO 179/1eA

    23 °C

    7 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m²

    dry

    ISO 179/1eA

    Impact strength, Charpy unnotched

    No Break at 23 and -30°C

    dry

    ISO 179/1eU

    Thermal

    PropertyValueConditionTesting StandardComment

    Melting point

    222 °C

    Show Supplier Material materials with Melting point of 222 °C

    dry

    ISO 11357-1/-3

    10°C/min

    Technological properties

    Property
    Application areas

    Monofilaments