Rilsan® 7310 Grey AC FB Fluid Bed Powder

Rilsan® fluid bed powders are thermoplastic polyamides obtained from renewable resources. Outstanding characteristics: abrasion resistance, corrosion resistance, impact resistance, sound reduction, flexibility, low coefficient of friction.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTesting StandardComment

Density

1.06 g/cm³

Show Supplier Material materials with Density of 1.06 g/cm³

ISO 1183

relative density

Fluidized density

0.5 [-]

Show Supplier Material materials with Fluidized density of 0.5 [-]

Median particles size

100 - 130 μm

Show Supplier Material materials with Median particles size of 100 - 130 μm

ISO 13320

Non Tap density

0.52 g/cm³

Show Supplier Material materials with Non Tap density of 0.52 g/cm³

ISO 1068

Tap density

0.62 g/cm³

Show Supplier Material materials with Tap density of 0.62 g/cm³

ISO 1068

Water absorption

1 %

Show Supplier Material materials with Water absorption of 1 %

ISO 62-1

max. | for 24h

Mechanical

PropertyValueTesting StandardComment

Hardness, Persoz

250 [-]

Show Supplier Material materials with Hardness, Persoz of 250 [-]

ISO 1522

Impact energy, coating

2 J

Show Supplier Material materials with Impact energy, coating of 2 J

ASTM G26

min.

Thermal

PropertyValueConditionTesting Standard

Melting point

183 - 188 °C

Show Supplier Material materials with Melting point of 183 - 188 °C

dry

ISO 1218

Electrical

PropertyValueTesting StandardComment

Dielectric strength

30 kV/mm

Show Supplier Material materials with Dielectric strength of 30 kV/mm

ASTM D149

thickness = 350-450mm

Technological properties

Property
Application areas

Powder Coatings - General Purpose

Color

Grey

Covering efficiency

0.33 kg/m²

Covering efficiency, thickness

300 µm