Rilsan® TECHLINE WHITE 7601

Alternative and trade names
PA11
Want to keep this datasheet? Save it now in your required format

Description

Rilsan® 7601 Techline White Minicoat/ Maxicoat Powder

Rilsan® minicoat/ maxicoat powders are thermoplastic polyamides obtained from renewable resources. Outstanding characteristics: abrasion resistance, corrosion resistance, impact resistance, sound reduction, flexibility, low coefficient of friction.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Abrasion resistance, weight loss

8 mg

Show Supplier Material materials with Abrasion resistance, weight loss of 8 mg

ISO 9352, Wheel CS 17, load 1 kg, 1000 cycles

Median particles size

30 - 60 μm

Show Supplier Material materials with Median particles size of 30 - 60 μm

ISO 13320

Non Tap density

23.0 °C

0.44 g/cm³

Show Supplier Material materials with Non Tap density of 0.44 g/cm³

ISO 1068

Relative density

23.0 °C

1.11 [-]

Show Supplier Material materials with Relative density of 1.11 [-]

ISO 1183

Tap density

23.0 °C

0.57 g/cm³

Show Supplier Material materials with Tap density of 0.57 g/cm³

ISO 1068

Water absorption

23.0 °C

1 %

Show Supplier Material materials with Water absorption of 1 %

max., ISO 62-1, 24h

Mechanical

PropertyValueComment

Hardness, Persoz

270 [-]

Show Supplier Material materials with Hardness, Persoz of 270 [-]

ISO 1522

Thermal

PropertyValueComment

Melting point

183 - 188 °C

Show Supplier Material materials with Melting point of 183 - 188 °C

ISO 1218

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

10 kV/mm

Show Supplier Material materials with Dielectric strength of 10 kV/mm

ASTM D149, thickness = 100mm

Technological properties

Property
Application areas

Main applications:

  • Coating of small items such as undergarment clips
  • fasteners
  • small automotive parts
  • stamped metal
  • and boot eyelets
  • Rilsan® minicoat/ maxicoat powders are designed to coat small parts with metal substrates via the minicoat or maxicoat process. The Techline White grade is designed for further pigmentation to create a wide spectrum of colors
  • Powder Coatings For General Purpose and Undergarments

  • Color

    White

    Covering efficiency

    0.22 kg/m²

    Covering efficiency, thickness

    200 µm

    Other

    Additional info:

  • Smooth texture with a glossy appearance
  • Good adhesion after over 2000 hours of salt spray testing (ISO 9227)
  • Only 10% fine particles < 20 µm (ISO 13320)
  • Only 6% coarse particles > 80 µm (ISO 13320)
  • 5 year shelf life from date of manufacture
  • Available in 20 kg bags- For more information visit: www.rilsanfinepowders.com