Description

Rilsan® TIEFLEX S452 NAT T6L resin is a flexible tie layer alloy partially based on renewable resources. This grade is designed for multilayer automotive and trucks lines (tie layer for fuel line). In the case of direct contact with fuel, contact Arkema representative for recommendations.

Packaging:

This grade is delivered dried in sealed packaging (25kg bags) ready to be processed.

Shelf life:

Two years from the date of delivery. For any use above this limit, please refer to our technical services.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.09 g/cm³

Show Supplier Material materials with Density of 1.09 g/cm³

dry

ISO 1183

Moisture absorption

1.2 %

Show Supplier Material materials with Moisture absorption of 1.2 %

Sim. to ISO 62

Water absorption

2.9 %

Show Supplier Material materials with Water absorption of 2.9 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.515 GPa

Show Supplier Material materials with Elastic modulus of 0.515 GPa

cond.

ISO 527-1/-2

0.685 GPa

Show Supplier Material materials with Elastic modulus of 0.685 GPa

dry

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min. | nominal

Elongation at yield

31 %

Show Supplier Material materials with Elongation at yield of 31 %

cond.

ISO 527-1/-2

Impact strength, Charpy notched

-30 °C

6.5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6.5 kJ/m²

cond.

ISO 179/1eA

23 °C

95 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 95 kJ/m²

cond.

ISO 179/1eA

Impact strength, Charpy unnotched

No Break at 23 and -30°C

cond.

ISO 179/1eU

Thermal

PropertyValueConditionTesting StandardComment

Melting point

217 °C

Show Supplier Material materials with Melting point of 217 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

3.7 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 3.7 cm³/10min

dry

ISO 1133

235°C/5kg

Technological properties

Property
Application areas

Fuel Management - In-Tank and Fuel Venting Lines

Processing methods

Extrusion:

  • Typical melt temperature (min / recommended / max): 220°C / 230°C / 270°C
  • Drying time and temperature (only necessary for bags opened for more than two hours): 4-6 hours at 80°C