Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 25 % Show Supplier Material materials with Elongation of 25 % |
Elongation A50 | 23.0 °C | 23 % Show Supplier Material materials with Elongation A50 of 23 % |
Hardness, Brinell | 23.0 °C | 20 [-] Show Supplier Material materials with Hardness, Brinell of 20 [-] |
Tensile strength | 23.0 °C | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa |
Yield strength Rp0.2 | 23.0 °C | 20 MPa Show Supplier Material materials with Yield strength Rp0.2 of 20 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 99.5 % Show Supplier Material materials with Aluminium of 99.5 % |
Copper | 0.05 % Show Supplier Material materials with Copper of 0.05 % |
Iron | 0.4 % Show Supplier Material materials with Iron of 0.4 % |
Magnesium | 0.05 % Show Supplier Material materials with Magnesium of 0.05 % |
Manganese | 0.05 % Show Supplier Material materials with Manganese of 0.05 % |
Other | 0.03 % Show Supplier Material materials with Other of 0.03 % |
Silicon | 0.25 % Show Supplier Material materials with Silicon of 0.25 % |
Titanium | 0.05 % Show Supplier Material materials with Titanium of 0.05 % |
Zinc | 0.07 % Show Supplier Material materials with Zinc of 0.07 % |
Technological properties
Property | ||
---|---|---|
Coating | suitable for electro-chemical brightening and anodizing | |
Corrosion properties | corrosion resistant | |
Processing methods | Excellent forming properties | |
Welding | weldable |