General
Property | Value | Temperature | Comment |
---|---|---|---|
Bulk density | 6.11 g/cm³ Show Supplier Material materials with Bulk density of 6.11 g/cm³ at 23.0 °C | 23.0 °C | |
Particle size | 30 - 100 nm Show Supplier Material materials with Particle size of 30 - 100 nm | BET | |
Specific surface area | 15 - 30 m²/g Show Supplier Material materials with Specific surface area of 15 - 30 m²/g | BET |
Technological properties
Property | ||
---|---|---|
Application areas | proton conductor, solid oxide fuel cell, SOFC, solid electrolyte, ceramic membranes, protonic ceramic oxide fuel cell, oxide ion conductor, conductive solid electrolyte, proton ceramic electrolyzer cell, protonic ceramic membrane, proton conducting perovskite oxide, catalyst support | |
Chemical composition | BaZr0.8Y0.2O3-δ | |
Color | Fine, white powder | |
Crystal structure | Crystal structure at 25°C: Cubic perovskite, Pm-3m | |
Processing history | Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices. |