General
Property | Value | Temperature | Comment |
---|---|---|---|
Bulk density | 7.21 g/cm³ Show Supplier Material materials with Bulk density of 7.21 g/cm³ at 23.0 °C | 23.0 °C | |
Particle size | 30 - 100 nm Show Supplier Material materials with Particle size of 30 - 100 nm | BET | |
Specific surface area | 10 - 25 m²/g Show Supplier Material materials with Specific surface area of 10 - 25 m²/g | BET |
Technological properties
Property | ||
---|---|---|
Application areas | ceramic membranes, barrier layer SOFC, SOFC, solid oxide fuel cell, oxygen separation membranes, solid electrolyte, electronic conductor, membrane reactor, oxygen ionic transport membrane, dual-phase membrane, hydrogen separation membrane, cathode SOFC, protective layer SOFC, oxygen sensor | |
Chemical composition | Ce0.8Gd0.2O2-δ | |
Color | Fine, pale yellow powder | |
Crystal structure | Crystal structure at 25°C: Cubic flourite, Fm-3m | |
Processing history | Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices. |