Description

LNO is supplied as fine, black submicron powder with a chemical purity > 99% (Phase pure by XRD) and a primary particle size of 50-170nm (BET).

This material data has been provided by Cerpotech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTemperatureComment

Bulk density

7.03 g/cm³

Show Supplier Material materials with Bulk density of 7.03 g/cm³ at 23.0 °C

23.0 °C

Particle size

50 - 170 nm

Show Supplier Material materials with Particle size of 50 - 170 nm

BET

Specific surface area

5 - 15 m²/g

Show Supplier Material materials with Specific surface area of 5 - 15 m²/g

BET

Technological properties

Property
Application areas

capacitor, supercapacitor, electrode, anode, catalyst

Chemical composition

La2NiO4+δ

Color

Fine, black powder

Crystal structure

Crystal structure at 25°C: Ruddlesten-Popper layered structure, tetragonal I4/mmm

Processing history

Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices.