General
Property | Value | Temperature | Comment |
---|---|---|---|
Bulk density | 7.03 g/cm³ Show Supplier Material materials with Bulk density of 7.03 g/cm³ at 23.0 °C | 23.0 °C | |
Particle size | 50 - 170 nm Show Supplier Material materials with Particle size of 50 - 170 nm | BET | |
Specific surface area | 5 - 15 m²/g Show Supplier Material materials with Specific surface area of 5 - 15 m²/g | BET |
Technological properties
Property | ||
---|---|---|
Application areas | capacitor, supercapacitor, electrode, anode, catalyst | |
Chemical composition | La2NiO4+δ | |
Color | Fine, black powder | |
Crystal structure | Crystal structure at 25°C: Ruddlesten-Popper layered structure, tetragonal I4/mmm | |
Processing history | Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices. |