Barium iron zirconium cobaltite (BCFZ) Powder

Alternative and trade names
BFCZ, Barium iron zirconium cobaltite, iron- and zirconium substituted barium cobalt oxide, cobalt- and zirconium-doped barium ferrite
Want to keep this datasheet? Save it now in your required format

Description

BCFZ is supplied as fine, black submicron powder with a chemical purity > 99% (Phase pure by XRD).

This material data has been provided by Cerpotech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Technological properties

Property
Application areas

Solid oxide fuel cell, SOFC, Protonic cathode for SOFC, oxygen permeable membrane, protonic ceramic fuel cell, protonic conductor, electrode, SOEC, solid oxide electrolyser cell, electrocatalyst,

Chemical composition

BaCo0.4Fe0.4Zr0.2O3-δ

Color

Fine, black powder

Processing history

Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices.