Lanthanum tungstate (LWO) Powder

Alternative and trade names
Lanthanum tungstate
Want to keep this datasheet? Save it now in your required format

Description

LWO is supplied as fine, black submicron powder with a chemical purity > 99% (Phase pure by XRD).

This material data has been provided by Cerpotech.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Technological properties

Property
Application areas

mixed electron-proton conductor, SOFC, solid oxide fuel cell, photocatalyst, gas separation membrane, proton conductor, electrocatalyst, absorbent for heavy metal removal

Chemical composition

La5.4WO11+δ

Color

Fine, black powder

Processing history

Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices.