General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 17 g/cm³ Show Material materials with Density of 17 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 310 GPa Show Material materials with Elastic modulus of 310 GPa |
Elongation | 23.0 °C | 2 % Show Material materials with Elongation of 2 % |
Hardness, Rockwell C | 23.0 °C | 32 [-] Show Material materials with Hardness, Rockwell C of 32 [-] |
Tensile strength | 23.0 °C | 648 MPa Show Material materials with Tensile strength of 648 MPa |
Yield strength | 23.0 °C | 517 MPa Show Material materials with Yield strength of 517 MPa |
Chemical properties
Property | Value |
---|---|
Tungsten | 90 % Show Material materials with Tungsten of 90 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of Tungsten Alloys: Radiation shielding, boring bars, counterweights in aircraft and racing cars |