Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Gold 18 kt 3N
Yellow gold alloy
This material data has been provided by EPoS.
All categories
General
Property | Value |
---|---|
Density | 15.45 g/cm³ Show Supplier Material materials with Density of 15.45 g/cm³ |
Technological properties
Property | ||
---|---|---|
Other | Upon request. | |
Processing methods | E-Forged™ from powders |