General
Property | Value |
---|---|
Density | 2.45 g/cm³ Show Supplier Material materials with Density of 2.45 g/cm³ |
Porosity | 1 % Show Supplier Material materials with Porosity of 1 % |
Mechanical
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 7.7e-06 - 1.02e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.7e-06 - 1.02e-05 1/K |
Technological properties
Property | ||
---|---|---|
Other | Diameter 10 mm by 2-10 mm disks. Diameter 15 mm by 2-10 mm disks 20 x 10 x 2 to 6 mm heigh. Special shapes upon request. | |
Processing methods | E-Forged™ from powders |