General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Density of 2.66 g/cm³ |
Surface roughness | 15 μm Show Supplier Material materials with Surface roughness of 15 μm |
Dimension
Property | Value |
---|---|
Width | 1520 mm Show Supplier Material materials with Width of 1520 mm |
Dimensions | Standard stock sizes: 1520mm x 3020mm, 1570mm x 3670mm, 2160mm x 4000mm and 20-1070mm in thickness |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 70 GPa Show Supplier Material materials with Elastic modulus of 70 GPa | |
Elongation A5 | 23.0 °C | 10 - 15 % Show Supplier Material materials with Elongation A5 of 10 - 15 % | |
Hardness, HBW | 23.0 °C | 68 - 75 [-] Show Supplier Material materials with Hardness, HBW of 68 - 75 [-] | Test method: 2.5/62.5 |
Tensile strength | 23.0 °C | 230 - 290 MPa Show Supplier Material materials with Tensile strength of 230 - 290 MPa | |
Yield strength Rp0.2 | 23.0 °C | 110 - 130 MPa Show Supplier Material materials with Yield strength Rp0.2 of 110 - 130 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.33E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.33E-5 1/K |
Specific heat capacity | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 900 J/(kg·K) |
Thermal conductivity | 23.0 °C | 110 - 130 W/(m·K) Show Supplier Material materials with Thermal conductivity of 110 - 130 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.60E+7 - 1.80E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.60E+7 - 1.80E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: O3, homogenized and stress relieved |