General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.85 g/cm³ Show Supplier Material materials with Density of 2.85 g/cm³ |
Dimension
Property | Value |
---|---|
Dimensions | Standard stock sizes: 3000mm and 10-300mm in thickness |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 70 GPa Show Supplier Material materials with Elastic modulus of 70 GPa | |
Elongation A5 | 23.0 °C | 6 - 8 % Show Supplier Material materials with Elongation A5 of 6 - 8 % | |
Hardness, HBW | 23.0 °C | 95 [-] Show Supplier Material materials with Hardness, HBW of 95 [-] | Test method: 2.5/62.5 |
Tensile strength | 23.0 °C | 330 - 370 MPa Show Supplier Material materials with Tensile strength of 330 - 370 MPa | |
Yield strength Rp0.2 | 23.0 °C | 210 - 250 MPa Show Supplier Material materials with Yield strength Rp0.2 of 210 - 250 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.3E-5 1/K |
Specific heat capacity | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 900 J/(kg·K) |
Thermal conductivity | 23.0 °C | 130 - 160 W/(m·K) Show Supplier Material materials with Thermal conductivity of 130 - 160 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.80E+7 - 2.20E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.80E+7 - 2.20E+7 S/m |
Technological properties
Property | ||
---|---|---|
Processing history | Temper: T4, T4510, T4511 |