Alloy EN AW 6082 (AlSi1MgMn), situated in the upper segment of medium-strength rolled plates, has very good resistance to stress corrosion cracking (SCC) in addition to high thermal conductivity.

Related Standards

Properties

General

Density ρ

2.7 g/cm³ at 20 °C

Dimension

Dimensions

Standard stock sizes: 1520mm x 3020mm and 3-100mm in thickness

Mechanical

Elastic modulus E

70 GPa at 20 °C

Elongation A50 A50

7 - 10 % at 20 °C

Hardness, HBW HBW

89 - 94 [-] at 20 °C

Test method: 2.5/62.5

Tensile strength Rm

295 - 310 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

240 - 260 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.34E-5 1/K at 20 °C

Specific heat capacity cp

896 J/(kg·K) at 20 °C

Thermal conductivity λ

170 - 220 W/(m·K) at 20 °C

Electrical

Electrical conductivity σel

2.40E+7 - 3.20E+7 S/m at 20 °C

Technological properties

Other

Heat treatable alloy

Processing history

Temper: T6, T651

This material data has been provided by Gleich Aluminum.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.